Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_7210 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_7220 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_7230 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroClear FullCure810 Information provided by Proto3000 for their protoyping engineering services. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 50.0 °C | 117 - 122 °F | ASTM D648-98c |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |