Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | |
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | |
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | |
LATI Larton L G/40 L-PPS, 40% Glass Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | |
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | |
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | |
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | |
LATI Latilub 57D-15T G/30 PPA, 30% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C @Thickness 3.20 mm |
536 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPS 0334 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPS F GF/M55 BK 55% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features include : Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 280 °C | 536 °F | |
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |