Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C @Thickness 6.35 mm |
532 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ SF-30CF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched (Europe-Africa-Middle East) LNP* Lubricomp* OCL4036 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C @Thickness 3.20 mm |
532 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C @Thickness 3.20 mm |
532 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP OX91041 PPS - LINEAR (Europe-Africa-Middle East) LNP* LUBRICOMP* OX91041 is a compound based on PPS Linear resin containing Carbon Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp OC008A PPS - Branched LNP* Thermocomp* OC008A is a compound based on Branched Polyphenylene Sulfide containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East) LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | ISO-R 75 Method B |
Hippe PAI Polyamide-imide Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, fl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | ASTM D648 |
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)
(discontinued Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 278 °C | 532 °F | ASTM D648 |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |