Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled
(discontinued **) AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (DAM)
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 - 280 °C | 475 - 536 °F | Average value: 262 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PET GF20 UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ISO 75-1/-2 |
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS BKB085 is a 14% glass reinforced toughened heat stabilized black polyamide 66 resin.Information provided by DuPont Performanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
Ashley Polymers Ashlene® 528L-25G Nylon 66, 25% Glass Reinforced General purpose glass reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
Ashley Polymers Ashlene® 541-33G Nylon 66, 33% Glass Reinforced Nylon 66, 33% glass reinforced for extrusion applications.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
Ashley Polymers Ashlene® 520-25G Nylon 66, 25% Glass Reinforced Nylon 66, 25% glass reinforced.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 246 °C | 475 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |