Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ISO 75, ASTM D648 |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ISO 75, ASTM D648 |
Nilit Nilitop BT G6 FR C3 is a 30% Glass Fiber Reinforced, Flame Retardant PBT Description: Nilitop BT G6 FR C3 is a 30% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | Unannealed, Conditioned; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6 Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C @Thickness 3.20 mm |
430 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C @Thickness 3.20 mm |
430 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFP36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Silicone. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ASTM D648 |
SPS Guang Zhou POBUXâ„¢ 3001EPG20 Non-halogen flame retardance/GF20%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C @Thickness 3.20 mm |
430 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C @Thickness 3.20 mm |
430 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP WF006L PBT LNP* THERMOCOMP* WF006L is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C @Thickness 3.20 mm |
430 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ASTM D648 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ASTM D648 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ISO 75-1/-2 |
DuPont Performance Polymers Crastin® HR5330HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ASTM D648 |
Clariant Renol PBTG30-L Polybutylene Terephthalate, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ISO 75-1/-2 |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP JF002R PES (Europe-Africa-Middle East) LNP* Thermocomp* JF002R is a compound based on Polyethersulfone resin containing Glass Fiber, Glass Bead. Added features of this material include: Mold Release. |