Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Nylene® Vexel™ B12GF45 , 45% Glass Reinforced PBT Description: Vexel™ B12GF45 is a 45% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Polymer Resources NY6-G50 Nylon 6, 50% Glass Reinforced Nylon 6, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0135 BL069 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 CF30 30% Carbon Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAppearance: Black and Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF HS UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcements, 33% Filler by WeightAdditive: Lubricant, Heat Stabilizer and UV Stabilizer Features: Lubricated, Good UV Re.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF30 HF L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant Features: Lubricated and High FlowAppearance: BlackInformation provi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF30 HS L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF33 HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF33 HS L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF33 L RD041 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: YellowTPCI# 8221102Information provi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF33 L RD079 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: RedInformation provided by TP Compos.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPX-PBT-01055 60% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Filler, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6,6 109 L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Copolymer and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Plastics Group Polifil® 930L-13GF Glass Fiber-Reinforced Nylon 6 (DAM) Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in ind.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Chase Plastics CP Pryme® N233GL (DAM) Nylon 6, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Asahi Kasei Thermylon® NSG-240A-C 50% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Aaron Industries AAROPRENE® G/MFN 6002 Glass and Mineral Filled Nylon 6 AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA6 CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Conductive, Heat Stabilized and Lubric.. |