Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | Unannealed; ASTM D648 |
PolyOne Gravi-Tech™ GRV-NY-027-SS-BLK-F Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C @Thickness 3.20 mm |
370 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PSU TL20 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C @Thickness 3.20 mm |
370 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East) A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C @Thickness 3.20 mm |
370 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA (Asia Pacific) High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C @Thickness 3.20 mm |
370 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6) VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | 1/4 inch bar; ASTM D648 |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6) Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6) Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6PAM MoS2-Filled Cast Nylon 6 (PA6) Tecast® 6PAM is a molybdenum disulfide-filled cast nylon 6 used for general bearings and wear applications and for its superior strength and hardness.General Tecast® Cast Nylon Information: Tecast.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
ALM PA 850 Black Nylon 11 SLS Prototyping Polymer Information provided by Advanced Laser Materials (ALM). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ASTM D648 |
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | ISO 75 |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |