Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant Halogen and phosphor freeInformation provided by PolyPlastic Group. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Nilit FRIANYL A63 N-V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, low viscosity, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Nilit FRIANYL B63 V0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75-1/-2 |
DSM Akulon® F223-DH (Dry) Low/Medium Viscosity, Heat Stabilized Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | |
LATI Latistat 62-08 PA6 Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU (Asia Pacific) LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX CRN500 PPE+PA6 (Asia Pacific) Pa6 based unfilled GTX for Non-Auto marketThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL GTX GTX963 PPE+PA (Europe-Africa-Middle East) NORYL GTX963 is an unfilled impact modified material with excellent heat properties and good processability. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 Conductive GTX, CTE 7 |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Polyram PlusTek PB142 Nylon 6 for Injection Molding General purpose, fast cycle Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | DIN 53461 |
Polyram PlusTek PB507 Nylon 6, Flame Retardant Flame retardant halogen free polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | DIN 53461 |
Polyram PlusTek PB500 Nylon 6, Flame Retardant Flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BS 23 PA6 Information provided by EMS Grivory |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | |
Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, 50% RH Neat resin, for injection molding.Information provided by Cresset Powers Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 4185 black 9453 PA* Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Starflam PX05004 PA66, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Starflam PK0052E PA6, 25% Mineral Filled, Injection Molded PK0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3520Z222 or PA 25E6 U9 Z22)Information provided by Polymer Technolo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75-1/-2 |
DSM Akulon® F223-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | ISO 75 |
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C @Thickness 3.20 mm |
365 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 185 °C | 365 °F | |
LATI Latimass 62-05 D040 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |