Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | ASTM D648 |
Nylene® 9110 Unfilled Nylon 6/10 Description: Nylene® 9110 is an unfilled specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | ASTM D648 |
PTS Trimid® N6-200L Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 3.20 mm |
345 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 3.20 mm |
345 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 3.20 mm |
345 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 3.20 mm |
345 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 3.20 mm |
345 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® XHT4143T PC Copolymer (Asia Pacific) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 3.20 mm |
345 °F @Thickness 0.126 in |
ASTM D648 |
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 3.20 mm |
345 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP HAL23 PA11 (Europe-Africa-Middle East) LNP* LUBRICOMP* HAL23 is a compound based on PA 11 resin containing Aramid Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/66 IM 6040 MB Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0254 C 75% Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium Sulfate, 75% Filler by WeightFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0303 B Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityAppearance: Natural Color and WhiteInformation provided by TP Composites, Inc... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 0146 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6,6 IM 6040 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | ISO 75 |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 6.40 mm |
345 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 6.40 mm |
345 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0232 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0390 S1 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0425 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | ISO 75-1/-2 |
Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | |
Covestro Apec® HT KU 1-9350 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Medical sector: superheated steam sterilization.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | |
Covestro Apec® HT KU 1-9351 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers, indicator and brake light lenses.Information provided by Bayer.As of 1 September 2015, Ba.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | ASTM D648 |
Ashley Polymers Ashlene® 735 Nylon 6 Economy grade, impact modified Nylon 6 for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | ASTM D648 |
Ashley Polymers Ashlene® 990L Nylon 610 A general purpose, medium viscosity grade for injection molding and extrusion.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 174 °C @Thickness 6.40 mm |
345 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |