Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ASTM D648 |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Europe-Africa-Middle East) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 - 179 °C | 340 - 355 °F | Average value: 177 °C Grade Count:5 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 IM 7040 MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 IM 7050 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 TSX10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 TSX15 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE+ Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6 NAT001 Nylon 6 Availability: North AmericaForms: PelletsFeatures: Good Processability and High FlowAppearance: NaturalTPCI# 1327102Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ASTM Test |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C @Thickness 3.20 mm |
340 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | method Bf; ISO 75-2 |
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 588P NC010 Acetal (POM) Nucleated Medium Viscosity Acetal HomopolymerInformation provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ASTM D648 |
Clariant Renol 6253 Nylon 6, High Impact Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ASTM D648 |
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ASTM D648 |
Adell BD-10 Nylon 6, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ASTM D648 |
Adell BD-30 Nylon 6, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ASTM D648 |
Ashley Polymers Ashlene® RH190-PF Acetal, PTFE Filled A wear-resistant grade homopolymer resin with 1.5% PTFE.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N2200 HL Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackProcessing Method: Injection MoldingInformation pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |