Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 312.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 156.0 °C
312.8 °F
ASTM D648
KEP Kepital® TX-31 Wear/Friction/Resistant Acetal Copolymer
Kepital® is a registered trademark of Korea Engineering Plastics Co., Ltd. Information provided by Dayson Polymers.