Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
RheTech Products F38-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Electrical housingsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 IM 409 L MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM CO GC20 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM 0212B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Plastics Group Polifil® GFPPCC-30 30% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® PC320R Polycarbonate, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P1-35FM-1374H 35% Glass/Fiber Reinforced Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-20FG-0600 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-20FG-2153 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-30FG-0708 30% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D648 |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |