Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | 267 °F | ASTM D648 |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | 267 °F | ASTM D648 |
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | 267 °F | ASTM D648 |
Westlake Plastics Pomalux® SD-A Acetal Copolymer (anti-static) Non-carbon-filled, permanently static-dissipative material which is non-migratory and non-humidity dependent. With enhanced lubricity, POMALUX SD-A provides superior wear resistance and ease of mac.. |