Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
RheTech Products M12P100-01 12% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPHC T5040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics GELOY HRA170 ASA (Europe-Africa-Middle East) GELOY HRA170 is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C @Thickness 3.20 mm |
250 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® ML7693 PC Copolymer (Asia Pacific) Medium-flow impact-modified high-flow-ductile PC copolymer. Available in black color only. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | Unannealed; ASTM D648 |
M. Holland Company PP100 Polypropylene Homopolymer, General Purpose High clarityHomopolymerGood melt strengthHigh tensile strengthApplications: Thin-walled partsSheetStrapping |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C @Thickness 6.40 mm |
250 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Fiberfil® PP-60/CC/30 Polypropylene Homopolymer, 30% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Total PPH 3429 Polypropylene, Injection Molding Grade LTHA injection molding homopolymerLTHA - FINA 3429 is engineered with an LTHA additive system that gives excellent leach resistance in hot/wet environments that contain bleach and laundry detergents.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ISO 75-2 |
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications Xmod HF006SA is a high melt flow PP homopolymer with increased crystallinity, intended for injection molding. Xmod HF006SA is specifically developed for applications demanding a high surface appear.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Total PPH 3825 Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerEasy Flow - FINA 3825 exhibits exceptionally easy flow characteristics.FDA - FINA 3825 complies with all applicable FDA regulations for food contact applicatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Ecomass® 1080ZD93 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Ecomass® 1080ZD94 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Techn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Ecomass® 1080ZG90 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityMetal Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by T.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
Ecomass® 1850ZG92 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ISO-R 75 Method B |
Hippe PTFE Good chemical resistance. High thermal stability. Flame resistance. Lowest coefficient of friction among all solid plastics. Very good dielectric properties. Very high weathering resistance.Info.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 - 129 °C | 250 - 264 °F | |
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | |
Aaron Industries AAROPRENE® AE PC/ABS 7000-3 PC/ABS Engineered Resin Melt flow index may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 - 149 °C | 250 - 300 °F | Average value: 141 °C Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 °C @Thickness 3.20 mm |
250 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP.. |