Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS GF30 FR 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS E GM15 LE 15% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS E GM30 LE 30% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS E GM5 LE 5% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF15 BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 1018121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GM30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS WM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 9822121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF30 HT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF30 IM 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | ASTM D648 |
ExxonMobil PP1572 Polypropylene Homopolymer Product Description: A nucleated homopolymer resin designed for general-purpose compression molding of articles such as caps and closures. It exhibits excellent strength and high crystallization te.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | annealed; ASTM D-648 |
Axiall ProTherm® 4351 Rigid PVC, Extrusion Georgia Gulf ProTherm® 4351 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial grade pipe requiring high heat deflection temperatures and excellent chemical resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 112 °C | 233 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF15 A1 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |