Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYsan FL100 F35 SAN, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Reliance Industries Repol B550MN Polypropylene REPOL Polypropylene B550MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
PolyMirae Moplen HF524J BDDP Film Grade Polypropylene Moplen HF524J is the Addiform polypropylene. Compared to ordinary pelletized polypropylene, Addiform gives significant advantages in terms of improved productivity, better processing and lower energ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
PolyMirae Moplen HP524J BDDP Film Grade Polypropylene Moplen HP524J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP524J is a homopolymer particularly suitable for BOPP (Tender) fil.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
PolyMirae Moplen HP525J BDDP Film Grade Polypropylene Moplen HP525J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP525J is a homopolymer particularly suitable for Metallizable BOPP.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75A-1,-2 |
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Hyosung Topilene F501 PP F501 Extrusion General HomopolymerApplications:Flat yarnRopeBandCharacteristics:ProcessabilityInformation provided by Hyosung Corporation |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Hyosung Topilene F600 PP F600 Film Grade HomopolymerApplications: IPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Flint Hills P4C6S-193A Homopolymer Polypropylene Features: Clarified, high Slip and Controlled Rheology. Product does not contain animal derived components. Phthalate-free.Applications: Specialty Injection Molding. Excellent Mold ReleaseInfor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | |
Ineos ABS Lustran® H701 Medium heat resistance, high impact strength. ,Property data per ISO test methods. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | |
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C @Thickness 3.20 mm |
221 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP M7001XXH PP LNP* THERMOCOMP* M7001XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additves. Designed for touch surfaces in patient critical healthcare applications. Added f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene DescriptionPolyfort® FPP 1697HU is a high flow fortified polypropylene with high temperature dimensioned stability. It is stabilized for UV exposure and available in matched automotive color.Infor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Total PPH 3727W Polypropylene, High Performance Injection Molding Grade Balanced Properties TOTAL Polypropylene 3727W strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | DIN 53461 |
Polyram RamOfin PPC342M6 Polypropylene, 30% Mineral Filled 30% mineral filled, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Unannealed; ASTM D648 |
ExxonMobil AP03B Polypropylene Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Aclo Accuguard Polypropylene HP0369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | |
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade Injection moldingsData was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Aclo Accutech ABS ABS834G40L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Unannealed; ASTM D648 |
Teknor Apex Sinpolene FRF2074 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 - 215 °C | 221 - 419 °F | Average value: 166 °C Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75-2 |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | |
Ineos ABS NOVODUR® P2T ABS, Injection Grade
(discontinued **) Injection molding grade, very high heat resistance.Applications: Automotive industry, household appliances.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This g.. |