Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 3.20 mm |
199 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 8100 MFD High Impact Polystyrene
(discontinued **) STYRON 8100 MFD high impact polystyrene is designed for microfloppy diskettes (MFD) applications. It offers easy processing, coloring, abrasion resistance, impact strength, and high heat resistance... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | 4 mm thick;10.0 mm wide molded rod; ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
LyondellBasell Pro-fax 6301 Polypropylene Homopolymer, Flake Resin Primary Processing Method: Masterbatch/ConcentratesKey Features: general purpose polypropylene homopolymer flake resin, minimal stabilization, FDA acceptableApplications: compounding, concentrates, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
LyondellBasell Pro-fax 6523 Polypropylene Homopolymer, General Purpose Key Features: general purpose polypropylene homopolymer resin, stiff, high resistance to solvents, FDA acceptableApplications: automotive, hospital and institutional ware, housewares, general moldin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 6.40 mm |
199 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | |
Ineos ABS Lustran® 488 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Stat-kon FX99030 PE (Europe-Africa-Middle East) LNP * Stat-kon* FX99030 is a compound based on Polyethylene resin containing Carbon Powder. Added features include: Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 3.20 mm |
199 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ISO 75 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 6.40 mm |
199 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 6.40 mm |
199 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Unannealed; ASTM Data |
Styron Magnum™ 2645 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.8 °C | 199 °F | Unannealed; ASTM D648 |
Styron XU 73120.00 Polycarbonate Resin Overview: XU 73120.00 Experimental Polycarbonate Resin is a high flow ignition resistant PC blend that contains no chlorinated or brominated additives. This resin is specifically designed to offer e.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Annealed; ASTM D648 |
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ISO 75-2 |
Borealis HG430MO Polypropylene HG430MO is a polypropylene homopolymer intended for injection molding. This polymer product is characterized by a superior impact resistance. This grade has ductile failure in falling weight impact .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Tipco Tipcolene® FPT 10 - 10% Talc Reinforced Polypropylene Homopolymer 10% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Formosa Plastics Formolene® 6550A Thin Walled Injection Molding Polypropylene Impact CopolymerApplications: Housewares, containers and other rigid packaging.Formolene 6550A (DEVELOPMENTAL) is a medium impact, high flow, controlled rheology copolymer of polypropylene designed .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Cheng Yu Plastic VH823 Flame Retardant ABS, High Impact |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Cheng Yu Plastic VH825 Flame Retardant ABS, Medium Impact |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.8 °C | 199 °F | ISO 75-2/B |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Braskem H 107 Coating Polypropylene Description: H 107 is a ultra-high melt flow rate additivated homopolymer used for general purposes. Designed for extrusion coating. This product exhibits excellent processability, good melt stabili.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Braskem H 107 Injection Molding Polypropylene Applications: Thin-walled parts and easy mould filling. Information provided by Braskem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | D-648 |
Bapolene® 4042 Polypropylene, Fiber/Filament Grade Bapolene PP4042 is a fiber extrusion resin with excellent thermal and mechanical properties. This product meets FDA standards for food contact applications.Applications: Rope and twine, fibrillated.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Ashley Polymers Ashlene® P261WO PPO A general purpose V-2 and V-0 rated resin for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled Increased flex w/ living hinge propertiesCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be cus.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Braskem H 510 Bioriented Film Polypropylene Applications: Bioriented films for conversion; adhesive tapes; textile and food packing. Information provided by Braskem |