Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 88.3 °C | 191 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 615APR Polystyrene
(discontinued **) STYRON® 615 APR is a general purpose easy flow resin typically used for medical, pharmaceutical and thin-walled parts. It is an excellent resin for blending with K-Resin (K-Resin is a trademark of .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.3 °C | 191 °F | ASTM D648 |
ExxonMobil PP4712E1 Polymer Grade for Oriented Film Product Description: Easy processing grade primarily for oriented film applications.Availability: North America and South America Features:MetalizableUses: Industrial Applications Oriented FilmTo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.3 °C | 191 °F | ASTM D648 |
ExxonMobil PP4792E1 Polymer Grade for Oriented Film Product Description: Easy processing grade primarily for oriented film applications.Availability: North America Features:MetalizableUses: Oriented FilmPackagingTapeProcessing Method: Film Extrusi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.3 °C | 191 °F | ASTM D648 |
Americas Styrenics EB6400 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.3 °C | 191 °F | ASTM D648 |
Americas Styrenics EC6600 High Impact Polystyrene Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy.. |