Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® H6030 High Density Polyethylene ApplicationsALATHON H 6030 is a homopolymer that provides enhanced processability, excellent stiffness and short molding cycles. Typical applications include thin wall and deep-drawRegulatory Statu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade ALATHON L5008HP is a bimodal, high molecular weight, high density polyethylene resin with excellent processability designed to meet the high performance requirements of pressure pipe applications in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade Alathon L5040 is able to incorporate high levels of post consumer recycle and retain excellent bottle physical properties. This resin provides high ESCR and processing stability. Typical application.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® L5440 High Density Polyethylene ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ASTM D648 |
Ineos R01C-01 Polypropylene Random Copolymer This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® L5876 High Density Polyethylene, Blow Molding Grade ALATHON L5876 is designed for injection blow molding and extrusion blow molding applications where higher gloss than standard grades is required. Regulatory Status: L5876 meets the requirements of t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | unannealed (0.250 in); ASTM D648 |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C @Thickness 3.17 mm |
169 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C @Thickness 3.17 mm |
169 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C @Thickness 3.17 mm |
169 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ISO 75 |
Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene Nontoxic alternative to Lead (Pb), for shielding applicationsHigh Specific GravityCarbonyl Iron Filled Polypropylene Random Co-PolymerInformation provided by Technical Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | ISO 75-2/B |
ExxonMobil PP7033L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C | 169 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDH-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, water and fruit drinks. In a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Braskem Green PE SHE150 Blown Film Extrusion and Cast Film Extrusion High Density Polyethylene Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Rasc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM-D648 |
Braskem HC7260LS-L HDPE Injection Molding Polyethylene HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 109 Polypropylene, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM-D648 |
Braskem HE150 HDPE Monofilament Polyethylene Copolymer HE150 resin is a high-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It has been specially designed for the monofilament extrusion process and provides a good balan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Ineos J50-2000-119 HDPE HDPE J50-2000-119 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 - 130 °C | 169 - 266 °F | Average value: 107 °C Grade Count:36 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene Description: SHC7260 is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. The minimum biobased content of .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® 9301 High Density Polyethylene ApplicationsALATHON 9301is a high density resin designed for sheet extrusion and thermoforming. It exhibits very low sag and high stiffness.Regulatory StatusALATHON 9301 meets the requirements of F.. |