Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 73.3 °C | 164 °F | ASTM D648 |
Plaskolite Vivak PETG Sheet VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.1 °C | 164 °F | ASTM D648 |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.3 °C | 164 °F | ASTM D648 |
ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.3 °C | 164 °F | ASTM D648 |
ExxonMobil HDPE HD 6719.62 High Density Polyethylene Copolymer Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.3 °C | 164 °F | 0.125";; ASTM D648 |
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.5 °C | 164 °F | CP-TM-12 |
PolyOne Elastamax HTE 2101-1000 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |