Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648-95 |
Multibase Multi-Pro® 0505 RC Black 5.2% Glass Filled Polypropylene This product was specially designed for one customer's glass filled polypropylene application.Data provided by Multibase. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM E2092 |
NatureWorks® Ingeo™ 3801X Injection Grade PLA Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PE 1295 PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance bet.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 66.0 °C | 149 - 151 °F | ASTM D648 |
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Rod Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Sheet Polyslick UHMW Sheet exhibits the properties of excellent impact strength, abrasion resistance, low coefficient of friction, as well as very good chemical resistance. This industrial grade material .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Profile Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C @Thickness 6.40 mm |
149 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | DIN 53461; ASTM D648 |
Kolon KOPEL® KP3340 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648-82 |
Micropol Microcene MC121 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648 |
ScanTube MFA Tubing Information provided by ScanTube, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648 |
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding Borecene RM8342RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8342RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648 |
Borealis Borecene™ RM8343 Linear Polyethylene for Rotational Molding Borecene RM8343 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ASTM D648 |
Eastman Drystar 0827 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
DSM Arnitel® PB420 TPC-ET Blow Molding Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
DSM Arnitel® PL461 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 70.0 °C | 149 - 158 °F | ASTM D648-98c |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow UNIVAL™ DMDC-6145 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6145 NT 7 provides good parison stability, which contribu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 66.0 °C | 149 - 151 °F | ASTM D648 |
3D Systems Accura® Bluestone™ Plastic for SLA® Systems A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 70.0 °C | 149 - 158 °F | |
C.O.I.M. EXTER S® S 108 A Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 108 A: Resin for van.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
Barlog Plastics KEBAFLEX P D40.3 Polyester-Elastomer, Shore D40 TPC-ETInformation provided by BARLOG plastics GmbH. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-2 |
Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications Bormed HE7541-PH is a bimodal, natural, high-density polyethylene produced by the Borstar PE technology. Bormed HE7541-PH combines low volatiles with high Environmental Stress Crack Resistance (ESC.. |