Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 54.4 - 76.7 °C | 130 - 170 °F | ASTM D648 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA11 GB30 HS 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 54.5 °C | 130 °F | ASTM D648 |
ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formula.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 54.5 °C | 130 °F | ASTM D648 |
ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formula.. |