Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 67.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 63.0 - 67.0 °C
145 - 153 °F
ASTM D648-06
Proto3000 Objet RGD525 High Temperature Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.