Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 304 °C | 410 - 580 °F | Average value: 248 °C Grade Count:90 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |