Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 124 - 138 °C | 255 - 280 °F | Average value: 130 °C Grade Count:5 |
Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 95.0 - 138 °C | 203 - 280 °F | Average value: 124 °C Grade Count:7 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |