Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Network Polymers NPP 25-5001 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Network Polymers NPP 30-3500 NA Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs SN0 ABS Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Reliance Industries Repol H080EY Polypropylene REPOL Polypropylene H080EY is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 - 113 °C | 210 - 235 °F | Average value: 106 °C Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Ineos H01G-00 Polypropylene Homopolymer Grade H01G-00 is a polypropylene homopolymer for fiber, tape, and consumer applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.152.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648-97 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Lotte Chemical Titan TITANPRO® 6331 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ISO 75B |
Lucite International Diakon® Frost 902 70 Acrylic Polymer Information provided by Lucite International |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C @Thickness 3.20 mm |
210 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C @Thickness 3.20 mm |
210 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ISO 75 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C @Thickness 6.40 mm |
210 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® HP-0500 ABS, Unreinforced Heat Resistant ABS material that can mainly be used for the exterior material of household appliances etc.Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C @Thickness 6.40 mm |
210 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C @Thickness 6.40 mm |
210 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ISO 75 |
Styrolution Terblend® N NM-12 ABS/PA6 (Dry) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp MX05039 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MX05039 is a compound based on Polypropylene resin containing Mineral, colorant. Added features include : Heat- Stabilized, UV - Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Annealed; ISO 75-2A |
Total PSC 1450N High Heat Resistance Polystyrene 1450N is a high heat resistance, easy flowing crystal polystyrene for the production of thick insulation board. The low viscosity of this grade makes it particularly suitable for the production of .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Eastman Tritan MX711 Copolyester Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow This product is intended for thin-wall injection molding applications as well as low denier filament yarns, extrusion coating and specialty cast embossed film.Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Entec Hypro™ PPH-CC20 Natural Homopolymer Polypropylene, 20% Calcium Carbonate Filled Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ISO 75-1/-2 |
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer Key Features: fast crystallization shortens cycle times, excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive blow molded partsMeets FDA requir.. |