Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 1012 C Polypropylene Calcium Carbonate Filler, 12% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 1020 C Polypropylene Calcium Carbonate Filler, 10% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2514 XU Polypropylene Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.18 mm |
205 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.18 mm |
205 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Maxxam™ PPC-40C Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2510 XG Polypropylene Mineral Filled, 25% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Global GPP-2500 Polypropylene Impact Copolymer, Nucleated Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® HDPE C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveUL File Number: E157318Appearance: BlackTPCI# 9411115Information provided by TP Composites.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® HIPS 1000 FR-E Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® HIPS FR-1 Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® HIPS E SL5 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant (5%)Appearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | 0.250 inch; ASTM D648 |
TPI Porene® GA800TW High Gloss/Weather Resistant/Antistatic Grade ABS INJECTION MOLDING; ANTISTATIC; WEATHER RESISTANT. HOUSING OF ELECTRICAL APPLIANCES, e.g. ELECTRIC FAN, TELEPHONE, CALCULATOR, TOYSPorene® is a registered trademark of Thai Petrochemical Industry C.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.17 mm |
205 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A100 ABS Molding Resin Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
ExxonMobil PP8255E1 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Engineered Polymer Solutions ABS 550 Medium Impact. Natural and colors available. Medium gloss. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Aclo Accutech ABS ABS832G10L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D-648 |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Aclo Accucomp ABS ABS801V Automotive Approved Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 - 205 °C | 205 - 401 °F | Average value: 149 °C Grade Count:153 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |