Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PP 1380 PRE-ELEC PP 1380 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PR.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 3.20 mm |
199 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 3.20 mm |
199 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® EX58 ABS High impact ABS for sheet extrusion and blow molding applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 3.20 mm |
199 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 8100 MFD High Impact Polystyrene
(discontinued **) STYRON 8100 MFD high impact polystyrene is designed for microfloppy diskettes (MFD) applications. It offers easy processing, coloring, abrasion resistance, impact strength, and high heat resistance... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 - 93.9 °C | 199 - 201 °F | Average value: 93.2 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | |
Arkema Group Oroglas® DRT Acrylic, Impact Grade
(discontinued **) For extrusion and injection molding applications. OROGLAS DRT combines good thermal resistance with an excellent impact resistance.Key features : impact resistance: up to 10 times more impact-resis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CH020 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
BP Amoco Acctuf® 3143 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Sheet extrusion; Thick-wall Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injectio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
LyondellBasell Pro-fax 6301 Polypropylene Homopolymer, Flake Resin Primary Processing Method: Masterbatch/ConcentratesKey Features: general purpose polypropylene homopolymer flake resin, minimal stabilization, FDA acceptableApplications: compounding, concentrates, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ISO Method 75 |
LyondellBasell Astryn BA36GC Polypropylene Copolymer Key Features: conventional melt flow, medium modulus, UV-stabilized polypropylene copolymer, moderate stiffness, good impact resistance, low foggingApplications: seat valances, passenger assist hand.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 6.40 mm |
199 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Prevex BJAX PPE+PS Foamable resin. All properties at 10% density reduction; 0.250" thick specimens; improved productivity.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ISO 75 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 6.40 mm |
199 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Unannealed; ASTM Data |
Styron Magnum™ 2630 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Unannealed; ASTM Data |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 3.20 mm |
199 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ISO 75-2 |
Borealis BJ380MO Polypropylene Copolymer BJ380MO is a very high melt flow heterophasic copolymer with high/medium impact strength and stiffness. This grade is designed for high-speed injection molding and contains nucleating and antistatic.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Tipco Tipcolene® FPT 10 - 10% Talc Reinforced Polypropylene Homopolymer 10% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Braskem H 107 Coating Polypropylene Description: H 107 is a ultra-high melt flow rate additivated homopolymer used for general purposes. Designed for extrusion coating. This product exhibits excellent processability, good melt stabili.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Braskem H 107 Injection Molding Polypropylene Applications: Thin-walled parts and easy mould filling. Information provided by Braskem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Ashley Polymers Ashlene® P261WO PPO A general purpose V-2 and V-0 rated resin for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled Increased flex w/ living hinge propertiesCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be cus.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Buckeye Polymers BP RPP 1012 C Polypropylene, 10% Mineral Filled Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
Adell RZ-18 Copolymer Polypropylene, 40% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |