Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT4900-74UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C @Thickness 3.18 mm |
195 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Maxxam™ PPH-20C UV Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Ineos H04G-00 Polypropylene Homopolymer This is a controlled rheology general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of film and profile extrusion applications... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Ineos R12C-00 Polypropylene Random Copolymer Grade R12C-00 is a high clarity, medium flow rate random copolymer with low antistat for injection molding and stretch blow molding applications. This material meets the requirements of the U.S. Foo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1001A Antimicrobial Polypropylene Random Copolymer An approx. 10 melt Polypropylene random copolymer containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1002AF Food Grade Polypropylene Random Copolymer An approx. 10 melt Polypropylene random copolymer with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1002ARX Biocompatible Polypropylene Random Copolymer A biocompatible approx. 10 melt injection molding grade of Polypropylene random copolymer for healthcare applications.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1002ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer A biocompatible( approx. 10 melt Polypropylene random copolymer for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1005ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer A biocompatible approx. 10 melt Polypropylene random copolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM Test |
Styrolution Terblend® N NM-11 ABS/PA6 (Dry) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM Test |
Styrolution Terblend® N NM-19 ABS/PA6 (Dry) Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROL.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | unannealed; ASTM D648 |
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | Unannealed; ASTM Data |
Styron Magnum™ 9035 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Washington Penn Medium Impact Copolymer 20% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration Accesso.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Asahi Kasei Thermofil P-10CC-1417 10% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |