Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
SABIC PS 126 General Purpose Polystyrene for Injection Molding Product Description: General purpose Polystyrene PS 125 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and hi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
LyondellBasell Pro-fax 7531 Polypropylene Impact Copolymer Primary Processing Method: Injection Molding/ThermoformingKey Features: medium impact polypropylene copolymer resin for food packaging, FDA acceptable, low odor and low taste transfer, good cold imp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Flint Hills PP 23R2A Random Copolymer Polypropylene Random copolymer, radiation sterilization resistant, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: High contact clarity, non-blushing, toughness, impact, chemical.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | |
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 3.20 mm |
194 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON MX12407C PP LNP* STAT-KON* MX12407C is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Stratasys® ABS ABS is a strong, durable production-grade thermoplastic used across many industries. ABS is an ideal material for conceptual prototyping through design verification through direct digital manufactur.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | pressure unspecified; ASTM D648 |
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | 120°C per hour; ISO 75-2 |
Total PPC 9712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | 120°C per hour; ISO 75-2 |
Total PPC 9760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | 120°C per hour; ISO 75-2 |
Total PPC 2660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 2660 is a heterophasic copolymer. PPC 2660 is characterized by a low fluidity hence good melt strength to provide ease of processing and good manufactured article properti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | |
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sepa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Aclo Accucomp ABS ABS846HL High Flow Medium Impact Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | |
BASF Novolen® 2348 TC Polypropylene Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Braskem CP 191 Injection Molding Polypropylene Applications: Household; low temperature packing; frozen desserts packaging. Information provided by Braskem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Cheng Yu Plastic C1100 PC/ABS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Cheng Yu Plastic C6600F PC/ABS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC 15000 Polypropylene Copolymer Information provided by Polykemi AB |