Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | Unannealed; ASTM D648 |
LyondellBasell Pro-faxâ„¢ SD183 Polypropylene Copolymer Description: Pro-faxâ„¢ SD183 medium impact polypropylene copolymer resin is extremely resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hostacomâ„¢ CB189FC/1 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB189FC/1 medium melt flow, 1,300 MPa flexural modulus, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact, stiffne.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HIPS 484 GY Availability: North AmericaForms: PelletsAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Westlake Plastics HIPS High Impact Polystyrene HIPS is a low cost plastic material that is easy to machine and fabricate. It is often specified for low strength structural applications when impact resistance, machinability, and low cost are req.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ISO 75-2/B |
ExxonMobil PP1063L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
ExxonMobil PP8244E1 Polypropylene Homopolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes.Availability: North America Features:Bala.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | Unannealed; ASTM D648 |
Dow H349-02 Polypropylene Homopolymer Resin H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is des.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Aclo Accucomp ABS ABS802L High Impact Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Aclo Accucomp ABS ABS812L High Impact Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Aclo Accucomp ABS ABS881L Clear Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Aclo Accucomp ABS ABS810L Medium Impact Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437M10CL Mica Reinforced Coupled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Americas Styrenics MC3650 High Heat Crystal Polystyrene Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Ineos H03G-01 Polypropylene Homopolymer This is a homopolymer designed for tenter frame BOPP processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsFood packagingOverwrap.. |