Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ASTM D648 |
Ineos H03G-04 Polypropylene Homopolymer This is a polypropylene homopolymer for biaxially oriented polypropylene (BOPP) film and blow molding applications. This material meets the requirements of the U.S. Food and Drug Administration as .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ISO 75-2/B |
ExxonMobil PP1014H1 Polypropylene Homopolymer Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ISO 75-2/B |
ExxonMobil PP1064L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ISO 75-2/B |
ExxonMobil PP5032E3 Polypropylene Copolymer Product Description: A polypropylene homopolymer type designed for production of monofilaments, tapes for the textile industry, geo textiles, fibrillated tapes for ropes and twines in the packaging.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ISO 75-2/B |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | Unannealed; ASTM D648 |
Dow 560.00 Developmental Performance Polypropylene Polymer OverviewConsistent processabilityExcellent gloss before and after thermoformingUV stabilized for increased weatherabilityD 560.00 Performance Polymer is designed as a co-extrusion cap layer for extr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | Unannealed; ASTM D648 |
Dow 560.01 Developmental Performance Polypropylene Polymer OverviewConsistent processabilityHigh glossGood regrind stabilityContains U.V. stabilizers for increased weatherabilityD 560.01 Performance Polymer is intended for use in extrusion blow molding, she.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | Unannealed; ASTM D648 |
Dow 6D83K Polypropylene Random Copolymer Resin OverviewConsistent processabilityLow odor and taste transferHigh glossGood regrind stabilityContains clarifying additiveComplies with: U.S. FDA 21 CFR 177.1520 (c)3.2a, Canadian HPFB No ObjectionDOW.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | unannealed; ASTM D648 |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648 |
Dow 6D83K Polypropylene Resin DOW 6D83K is intended for use in extrusion blow molding processes where enhanced clarity is desired.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437W20L1 Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ASTM D648 |
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceExcellent clarityGood moldabilityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk organizersInfor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ASTM D648 |
Aclo Accucomp ABS ABS809SL Extrusion Grade |