Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 - 80.0 °C | 167 - 176 °F | after thermal post treatment procedure A; ASTM D648-06 |
Proto3000 Objet RGD525 High Temperature Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC 20000 Polypropylene Copolymer Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Regulatory StatusThe base resin LR 7320 meets t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
Kolon NOPLA® KE531 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
LyondellBasell Hifaxâ„¢ ETA-3131E Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processabilityApplications: molded.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75 |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C @Thickness 3.20 mm |
167 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific) LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
SCG Chemicals EL-Leneâ„¢ H5814J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-2 |
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade desig.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-2 |
Borealis RG460MO Polypropylene, Transparent Random Copolymer RG460MO is a specially modified transparent polypropylene random copolymer with high melt flow. and is designed for high-speed injection molding and contains nucleating and demolding additives. Pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | |
Polyplastics TOPAS® 8007 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Water adsorption is small and barrier properties are good, making this grade particularly suitable for package applications for products that dislike moisture. Grade 8007 has lower coefficient of el.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
Tipco Tipcolene® TPE-HMI TPE HMI - Impact Modified Polypropylene Copolymer Compound with High Flow, Soft Touch High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-1,-2 |
Topas Advanced Polymers TOPAS® 8007D-61 Cyclic Olefin Copolymer (COC) TOPAS® 8007D-61 is an externally lubricated version of our 8007 series of injection molding resins, targeting injection blow molding (IBM) and injection stretch blow molding (ISBM) applications. Li.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
Eastman Tenite 285A3R30018 Butyrate Natural, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-1/-2 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D-648 |
Axiall MP-6510 Rigid PVC, Molding Georgia Gulf MP-6510 is a maximum properties electrical grade PVC injection molding compound processing excellent strength and toughness. In addition, it has good processing stability and surface a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D-648 |
Axiall MP-6585 Rigid PVC, Molding Georgia Gulf MP-6585 is an electrical grade rigid vinyl injection molding compound processing good strength, stiffness, toughness, and flow. In addition, it has excellent processing stability and s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM-D648 |
Braskem GM8260 HDPE Blow Molding Polyethylene Homopolymer HDPE GM8260 is a high-density polyethylene homopolymer that has high molecular weight and was developed for the blow molding segment of large volumes. Its applications include: drums for lubricant .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | |
Addcomp PRIEX® 25095 Maleic Anhydride Grafted PP random copolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
Carmel Olefins CAPILENE® QM 45 F Propylene Random Copolymer Description: CAPILENE® QM 45 F is a slip and anti-block formulated random copolymer. It is characterized by high gloss and easy processing.Applications: CAPILENE® QM 45 F is suitable for cast u.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75 |
LyondellBasell Hifax™ ETA-3163 Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | annealed; ASTM D-648 |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |