Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 - 143 °C | 162 - 290 °F | Average value: 123 °C Grade Count:42 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
Ineos R01C-00 Polypropylene Random Copolymer Grade R01C-00 is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding, through it is clarifier/antistat additive combination. Applications that requi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® HDPE 8904 FR UV GY Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: GrayInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE 8904 UV GY Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
Spartech Solarex® SV Copolyester Sheet Description: Copolyester SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | unannealed (0.125 in); ASTM D648 |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
ExxonMobil PP9513 Polypropylene Homopolymer Product Description: A random copolymer resin designed for non-oriented film.Availability: North America Features:Controlled RheologyEthylene Oxide SterilizableUses: BagsCast FilmHeavy-duty BagsPac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DMDA-8904 NT 7 High Density Polyethylene Resin DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | Unannealed; ASTM D648 |
Dow R792-35RNA Polypropylene Random Copolymer Resin OverviewControlled rheology productConsistent processabilityContains clarifying additiveContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW R.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437C10L Calcium Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C | 162 °F | unannealed; ASTM D-648 |
Axiall 8607 Rigid PVC, Extrusion Georgia Gulf 8607 is a special purpose pelletized compound formulated for high impact, rigid extrusion profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |