Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Global PPC-0320 Standard Grade Polypropylene Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hifaxâ„¢ CB272 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB272 high melt flow, 900 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of rigidity and dime.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Spartech Marballoy Marbleized Thermoplastic Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Spartech Polylite Foamed Polyolefin Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Spartech PP7210 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Spartech SP-1510 Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Spartech Ultros SRP Co-Extruded Skid-Resistant PE Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | ASTM D648 |
Ecomass® 1850ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)RigidInformation provided by Technical Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C | 160 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DMDA-8940 NT 7 High Density Polyethylene Resin DOW DMDA-8940 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |