Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C | 156 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE A biocompatiblei fractional melt High Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C | 156 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C | 156 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C | 156 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE2-0202ARX Biocompatible, Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C | 156 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C | 156 °F | ISO 75-2/B |
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C | 156 °F | ASTM D648 |
ExxonMobil HDPE HD 6605.70 High Density Polyethylene Copolymer Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C | 156 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DMDA-8965 NT 7 High Density Polyethylene Resin DOW DMDA-8965 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 - 142 °C | 156 - 288 °F | Average value: 104 °C Grade Count:30 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |