Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | ASTM D648 |
Ineos B4020N1331 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | ASTM D648 |
Ineos B4020N1332 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DMDA-8980 NT 7 High Density Polyethylene Resin DOW DMDA-8980 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | Unannealed; ASTM D648 |
Dow DS6D81 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW DS6D81 Polypropylene Resin is intended .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648 |
Dow DS6D81 Polypropylene Resin DOW DS6D81 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | Unannealed; ASTM D648 |
Dow DS6D82 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D82 Polypropylene Resin is intended for use as a heat seal coati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648 |
Dow DS6D82 Polypropylene Resin DOW DS6D82 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 67.8 °C | 154 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437C10L1 Calcium Reinforced |