Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 47.2 °C | 117 °F | ASTM D648 |
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.2 °C | 117 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.2 °C | 117 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 47.2 °C | 117 °F | ASTM D648 |
Aclo Accucomp Polyethylene HD0205L High Density |