Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 241 °C | 466 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 241 °C @Thickness 3.20 mm |
466 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 241 °C | 465 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PET GF15 IM FR X 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Impact Modifier and Mold ReleaseFeatures: Flame Retardant, Good Mold Release and Impact Modi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 241 °C | 466 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 940 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene Terephthalate Rynite 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength stiffness and low warpage.Informatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 241 °C | 466 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Star L PA66 D91 PA66, Aramid Fiber Filled, Injection Molded Star L PA66 D91 is a PTFE lubricated, Aramid Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 241 °C | 465 °F | ASTM D648 |
Clariant Renol 6601M Nylon 66, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 241 °C | 465 °F | ASTM D648 |
Clariant Renol 6642 2% Moly Nylon 66, Extrusion Grade, 2% Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 241 °C | 466 °F | ASTM D648 |
Ashley Polymers Ashlene® 68MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced nylon offering excellent dimensional stability and rigidity.Data provided by the manufacturer |