Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Polymer Resources NY6-G50 Nylon 6, 50% Glass Reinforced Nylon 6, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 - 228 °C | 420 - 442 °F | Average value: 222 °C Grade Count:22 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ISO 75-1, -2 |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0135 BL069 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF30 HS L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF33 L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackTPCI# 8221102Information provid.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6,6 109 L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Copolymer and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C @Thickness 3.20 mm |
421 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA6 CF30 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: Conductive Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6 GF13 FR-N BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | ASTM D648 |
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
Adell AD-10 Nylon 66, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
Adell BL-18 Nylon 6, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
Ashley Polymers Ashlene® 126 PBT Polyester, 30% Glass Reinforced General purpose 30% glass reinforcement, natural. Colors will modify properties.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
Ashley Polymers Ashlene® 830L-30G Nylon 6, 30% Glass Reinforced A 30% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type materials.Data p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
Ashley Polymers Ashlene® 830LS-33G Nylon 6, 33% Glass Reinforced A 33% glass fiber reinforced and heat stabilized Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
BLUESTAR 201-G25202 PBT, 25% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Bf |
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |