Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANAMID 66.6 C22^E F Nylon 66/6, Modified Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75/2Bf |
Radici Radilon® AHS (dry) Nylon 66 General purposeInformation provided by Radici group. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75 |
Nilit FRIANYL B63 MG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | |
Covestro Apec® 2000 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C @Thickness 6.40 mm |
383 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PBT-T15 15% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | |
LATI Latilub 62-06GR PA6, Graphite Reinforced Self-lubricating product based on Polyamide 6 (PA6). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C @Thickness 6.40 mm |
383 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX951W PPE+PA66 (Asia Pacific) A new high flow GTX designed for under-the-hood applications such as power distribution boxes, relay boxes and junction boxes. Developmental name: EXNX0151. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM AUT200M PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C) with internal mold release.. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are re.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
Unitika A125 PA66, Dry Information provided by Unitika Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 195 °C @Thickness 3.20 mm |
>= 383 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 195 °C @Thickness 3.20 mm |
>= 383 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 195 °C @Thickness 3.20 mm |
>= 383 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 225 30% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 225 is an injection molding grade, 30% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | |
Covestro Baydur® GS PIR B Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
DSM Arnite® TM4 440 (PBT+PET)-MD20 20% Mineral Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Staramide BS6 PA6, 30% Glass Bead Filled, Injection Molded Staramide BS6 is a 30% Glass Bead Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ASTM D648 |
Clariant Renol PA101L Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ASTM D648 |
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75-1/2 |
Eurotec® Tecomid® NB40 NL XA 20 PA 6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75-2 |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75-2 |
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75-2/B |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | |
Radici Radilon® A 38 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | ISO 75-1/-2 |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |