Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Annealed; ISO 75-1/-2
DuPont Performance Polymers Crastin® CE2055 NC010 PBT  (Unverified Data**)
Crastin® CE2055 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Deflection Temperature at 0.46 MPa (66 psi) 184 °C

@Thickness 3.20 mm
363 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66
LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant.
Deflection Temperature at 0.46 MPa (66 psi) 184 °C

@Thickness 3.20 mm
363 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp GC006XXZ PSU
LNP THERMOCOMP* GC006XXZ is a compound based on Polysulfone resin containing Carbon Fiber.This product is also known as Thermocomp* GC-1006.This data was supplied by SABIC-IP for the Americas region..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C

@Thickness 3.20 mm
363 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp GF003 PSU
LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU (Europe-Africa-Middle East)
LNP* THERMOCOMP* GF006 is a compound based on Polysulfone resin containing Glass Fiber.
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT
LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer
LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber
Only opaque colors available, with 20% glass fiber reinforcement, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
Covestro Apec® HT KU 1-9363 High-Heat Polycarbonate, UV-Stabilized
Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
annealed; ISO 75-1/-2
DuPont Performance Polymers Crastin® CE2055 NC010 Polybutylene Terephthalate (PBT)
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Perf..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
ASTM D648
A. Schulman ComAlloy Lubrilon® 62S1 Internally Lubricated, Nylon 6/6
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
ASTM D648
ALM PA 620-MF Mineral Fiber Filled Nylon 12 SLS Prototyping Polymer
Information provided by Advanced Laser Materials (ALM).
Deflection Temperature at 0.46 MPa (66 psi) 184 °C
363 °F
ASTM D648
ALM PA 860 White Nylon 11 SLS Prototyping Polymer
Unfilled White PA 11 that is formulated for easy processing across all LS platforms. Tightly controlled particle distribution creates a smooth surface finish and excellent feature detail. Parts prod..
Deflection Temperature at 0.46 MPa (66 psi) 184 - 223 °C
363 - 433 °F
Average value: 214 °C Grade Count:39
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Copyright © lookpolymers.com All Rights Reserved