Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 242 °F | ASTM D648 |
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 3.20 mm |
243 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | |
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, As Conditioned
(discontinued **) Standard injection molding grade, easy flow, easy mold release, fast setting.Applications: Thin walled engineering parts. Automotive sector: air filters, switch and connector parts for car electric... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Flint Hills P4G4K-205 Homopolymer Polypropylene Features: Clarified material. Product does not contain animal derived components. Phthalate-free.Applications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 6.40 mm |
243 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 3.20 mm |
243 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl PKN4766 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High flow. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 3.20 mm |
243 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp ZF0041XC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF0041XC is a compound based on PPE+PS Blend resin containing Glass Fiber and Flame retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Euro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® BM7300THS BK317 Nylon 6
(Unverified Data**) Zytel® BM7300THS is an unreinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437M40CL Mica Reinforced Coupled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0336M10CL Mica Reinforced Coupled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 - 120 °C | 243 - 248 °F | |
C.O.I.M. EXTER S® S 402 Isophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 402: High-quality re.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0436T30L1 Talc Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPHC TS20040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Unannealed; ASTM D648 |
Styron EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGE™ PC/PET 9100 CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5652EM is an extrusion grade.Information provided by Samyang. |