Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANTEC PC 85FR Polycarbonate, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
PolyMirae Moplen HP524J BDDP Film Grade Polypropylene Moplen HP524J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP524J is a homopolymer particularly suitable for BOPP (Tender) fil.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 - 113 °C | 221 - 235 °F | Average value: 110 °C Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75A-1,-2 |
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Reliance Industries Repol B400MN Polypropylene REPOL Polypropylene B400MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Hyosung Topilene F301U PP F301U Extrusion General HomopolymerApplications: Heavy duty bagCharacteristics:ProcessabilityWeatherabilityHigh tenacityInformation provided by Hyosung Corporation |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Hyosung Topilene F400 PP F400 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Hyosung Topilene J340 PP J340 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Flint Hills P4C6Z-022 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Res.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Hyosung Topilene J640U PP J640U Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityWeatherabilityInformation provided by Hyosung Corporation |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
LG Chemical SEETEC H7411 Polypropylene, Homopolymer Features: Seetec H7411 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and U.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON AE004 ABS LNP STAT-KON* AE004 is a compound based on ABS resin containing 20% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East) NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL N110 PPE+HIPS (Europe-Africa-Middle East) NORYL N110 is an unfilled material, with a Vicat B/120 of 115 °C according ISO 306. NORYL N110 has medium temperature resistance and good |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75-1/-2 |
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Aclo Accutech ABS ABS834G30L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer HP0334W10L Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Carmel Olefins CAPILENE® HT 75 A Polypropylene Impact Copolymer Description: CAPILENE® HT 75 A is a nucleated and antistatic high flow impact copolymer for injection molding. It is characterized by improved stiffness, medium impact resistance and good organol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Cheng Yu Plastic B600 PC/PBT |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Asahi Kasei Thermylene® P1-20FG-2703 20% Glass Fiber Reinforced, Impact Modified Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Unannealed; ASTM D648 |
Teknor Apex Sinpolene FRF2074 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75-2 |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75 |
Polyram RamOfin PPC361T4 Polypropylene, 20% Mineral Filled 20% Mineral filled, heat resistant polypropylene for injection molding applications.Information provided by Polyram. |