Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
RheTech Products HP521-188 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9777 Medium Beige Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs T00 GF20 ABS, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC T1010 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C @Thickness 3.20 mm |
214 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | |
Ineos ABS Lustran® H607AS Contains antistatic additives,Property data per ISO test methods. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
Ineos H03G-02 Polypropylene This is a homopolymer designed for fiber and tape applications requiring low water carryover and low die build-up. This resin meets the requirements of the U.S. Food and Drug Administration as spec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
Ineos N00N-00 Polypropylene Impact Copolymer Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ISO 75-1/-2 |
Lanxess Pocan® DP CF 2200 000000 PBT+PC PBT+PC, non-reinforced, injection molding, flame retardant, impact modified, low tendency to warp |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ISO 75-1/-2 |
Styrolution Luran® 378 P Crystal Clear Transparent SAN Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | annealed; ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C @Thickness 3.20 mm |
214 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C @Thickness 3.20 mm |
214 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS CR X BK Availability: North AmericaForms: PelletsFeatures: Good Chemical ResistanceUses: Electrical PartsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66 LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C @Thickness 3.17 mm |
214 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 101 °C | >= 214 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ISO 75 |
Polyram RamShine PAS702 ASA, UV Stabilized UV stabilized, general purpose, injection molding ASA.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C @Thickness 3.17 mm |
214 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
Eastman Tritan TX1801 Copolyester, Natural Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
Aclo Accuguard Polypropylene CP0467V0CSL Copolymer Flame Retardant Copper Stabilized |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
Aclo Accutech ABS ABS833G20L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
Amco PRIMATOP PP HOMO 038X Fiber Grade Polypropylene PP HOMO 038X features low water carryover. Applications include woven fabric and bags, rope and cordage, woven carpet backing, and woven geotextile fabrics.Former A-Top Polymers product; part of Amc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
Braskem H 604 Thermoforming & Extrusion Polypropylene Homopolymer Transparent packaging for food; Flat and corrugated sheets for school and office folders.Information provided by Braskem. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
A. Schulman ComAlloy Comshield® 215 High Impact Polystyrene, Electrically Conductive - Carbon Black Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 °C | 214 °F | ASTM D648 |
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |