Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 150 °C @Time <=86400 sec |
302 °F @Time <=24.0 hour |
|
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Maximum Service Temperature, Air | 150 °C @Time 7.20e+7 sec |
302 °F @Time 20000 hour |
|
Murtfeldt Murinyl® Polyvinylidinefluoride As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur.. |
|||
Maximum Service Temperature, Air | 150 °C @Time 1.80e+7 sec |
302 °F @Time 5000 hour |
|
Murtfeldt Murylon® HT Nylon 46 The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir.. |
|||
Maximum Service Temperature, Air | 150 °C @Time <=86400 sec |
302 °F @Time <=24.0 hour |
|
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Maximum Service Temperature, Air | 150 °C @Time 7.20e+7 sec |
302 °F @Time 20000 hour |
IEC 60216/T1 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Maximum Service Temperature, Air | 150 °C @Time 7.20e+7 sec |
302 °F @Time 20000 hour |
IEC 60216/T1 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Maximum Service Temperature, Air | 150 °C @Time 7.20e+7 sec |
302 °F @Time 20000 hour |
IEC 60216/T1 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |