Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 550 °C @Time 1.80e+7 sec |
1020 °F @Time 5000 hour |
Inhomogeneous Heating |
Schott Nextrema® 724-5 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Maximum Service Temperature, Air | >= 550 °C @Time 1.80e+7 sec |
>= 1020 °F @Time 5000 hour |
Homogeneous Heating |
Schott Nextrema® 724-5 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Maximum Service Temperature, Air | 550 °C @Time 1.80e+7 sec |
1020 °F @Time 5000 hour |
Inhomogeneous Heating |
Schott Nextrema® 724-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |