Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 250 °C @Time <=180000 sec |
482 °F @Time <=50.0 hour |
IEC 60216/T1 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Maximum Service Temperature, Air | 250 °C @Time <=180000 sec |
482 °F @Time <=50.0 hour |
IEC 60216/T1 |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Maximum Service Temperature, Air | 250 °C @Time 1.80e+7 sec |
482 °F @Time 5000 hour |
|
Murtfeldt Murpec® Polyetheretherketone In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change.. |
|||
Maximum Service Temperature, Air | 250 °C @Time 1.80e+7 sec |
482 °F @Time 5000 hour |
|
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |