Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 13.0 °C @Time 7.20e+7 sec |
55.4 °F @Time 20000 hour |
IEC 60216/T1 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |