Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.5 - 16.5 µm/m-°C @Temperature 20.0 - 200 °C |
8.61 - 9.17 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
CTE, linear | 15.5 - 16.5 µm/m-°C @Temperature 20.0 - 200 °C |
8.61 - 9.17 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
CTE, linear | 15.5 - 16.5 µm/m-°C @Temperature 20.0 - 200 °C |
8.61 - 9.17 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |